Description
Evaporating Dishes, Flat Form, Porcelain
Shallow form with lip and flat bottom. Glazed except for rim and part of outside bottom.
Autoclavable. Withstand temperatures to 1150°C. To prevent thermal stress cracks, we strongly recommend a heating/cooling rate not exceeding 200°C per hour. United porcelain evaporating dishes offer excellent resistance to acids and alkalies except for hydrofluoric acid.
- Thermal Shock Resistance - average coefficient of expansion from 20° C to 200° C is 3.56 x 10-5, gradually increasing to 4.69 x 10-5 at 1050°C. Every batch of porcelain is heat tested in our factory.
- Glaze - No softening occurs up to 1000°C, and it is extremely white.
- Resistance to Chemical Action - Resistance to acids and alkalies is excellent, except for hydrofluoric acid.
Item # | Capacity (ml) | Top Outside Diameter (mm) | Quantity per pack |
---|---|---|---|
JEF035 | 35 | 65 | 6 |
JEF050 | 50 | 75 | 6 |
JEF080 | 80 | 85 | 6 |
JEF100 | 100 | 100 | 6 |
JEF200 | 200 | 120 | 6 |
JEF300 | 300 | 150 | 6 |